Material Notes:
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 131.03 MPa
19004 psi
ASTM D638
Elongation at Break >= 4.0 %
>= 4.0 %
ASTM D638
Flexural Strength 213.79 MPa
31008 psi
ASTM D790
Flexural Modulus 6.897 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 - 225 °C
410 - 437 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 204.44 °C
399.99 °F
ASTM D648