Lucas-Milhaupt Lithobraze 720 (BT) Silver Based Cadmium Free Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Lithobraze
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Lithobraze 720 (BT) Silver Based Cadmium Free Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Litho braze 720 is a good general purpose, low temperature filler metal of high fluidity for fluxless furnace brazing of stainless steels when used in dry hydrogen or inert atmospheres. Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.67 g/cc
0.349 lb/in³
Thermal Properties Metric English Comments
Melting Point 760 °C
1400 °F
Solidus 760 °C
1400 °F
Melting Point
Liquidus 760 °C
1400 °F
Flow Point
Component Elements Properties Metric English Comments
Copper, Cu >= 27.2 %
>= 27.2 %
Lithium, Li 0.25 - 0.50 %
0.25 - 0.50 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 71.15 - 72.15 %
71.15 - 72.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000339 ohm-cm

@Diameter 0.762 mm
0.00000339 ohm-cm

@Diameter 0.0300 in
annealed wire with 0.22% Li
Descriptive Properties Value Comments
Color Silver-White
Users viewing this material also viewed the following: