Material Notes:
Applications: Easy-Flo 30 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue strength and ability to make leak-tight joints where close clearances cannot be maintained, they have been widely used in the refrigeration and air-conditioning industry. Additional uses for these filler metals are tubular bicycle and furniture frames, where joint fitup may be variable. Characteristics: Easy-Flo 30 is a low temperature, economical, brazing filler metals capable of bridging gaps where poor joint fitup cannot be avoided. This filler metal has a tendency to liquate (i.e., separate into low and high melting constituents) when heated slowly and therefore it is preferable to use them where the heat source is sufficient to raise the part temperature rapidly through the melting range of the brazing filler meta. Handy Flux is recommended for use with this filler metal.Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-2a, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-2aInformation provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.09 g/cc
0.328 lb/in³
Thermal Properties Metric English Comments
Melting Point 607.2 - 710 °C
1125 - 1310 °F
Solidus 607.2 °C
1125 °F
Melting Point
Liquidus 710 °C
1310 °F
Flow Point
Component Elements Properties Metric English Comments
Cadmium, Cd 19 - 21 %
19 - 21 %
Copper, Cu 26 - 28 %
26 - 28 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 29 - 31 %
29 - 31 %
Zinc, Zn 21 - 25 %
21 - 25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000518 ohm-cm
0.00000518 ohm-cm