Lucas-Milhaupt Black Flux Silver Brazing Flux

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Black Flux Silver Brazing Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black Flux is a water base paste consisting of potassium salts of boron and fluorine. It is recommended for use with torch, induction, furnace, resistance, and other heating methods.AdvantagesNo grittinessCreamy consistencyFlux can be applied by brush, dip, or pneumaticProtection against parts and flux life during heating are excellentVertical adherence as applied is excellentFlux can be used as concentrated, heat diluted, or water dilutedInformation provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
pH 9.0
9.0
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 982 °C
1800 °F
Minimum Service Temperature, Air 593 °C
1100 °F
Descriptive Properties Value Comments
Composition Potassium salts of boron and fluorine
Dilution Water (60cc/lb)
Heat 150-170F
Type Paste - Particle size #325 mesh or finer