Material Notes:
Applications and Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is desired. This alloy offers good corrosion resistance properties and is generally used where temperature requirements are critical.Joint clearances of 0.1 to 0.15mm (.003 to .005 in) are optimum, but larger variations can still produce sound joints. Flux is required and proper selection will depend upon base metals to be joined. Specifications:This alloy conforms to the following specification: ASTM 60B, B32 SN60 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Specific Gravity 8.67 g/cc
8.67 g/cc
Thermal Properties Metric English Comments
Melting Point 182 - 191 °C
360 - 375 °F
Solidus 182 °C
360 °F
Melting Point
Liquidus 191 °C
375 °F
Flow Point
Component Elements Properties Metric English Comments
Lead, Pb 39.5 - 40.5 %
39.5 - 40.5 %
Tin, Sn 59.5 - 60.5 %
59.5 - 60.5 %
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: