Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD)

Category Polymer , Thermoset , Polydicyclopentadiene (PDCPD)
Manufacturer Lubrizol (former Noveon)
Trade Name Telene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® results in a polymer showing a unique combination of stiffness and high impact resistance, as well as good thermal properties. Telene® is self-demolding without any need for release agents.Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D 792
Brookfield Viscosity 310 - 390 cP

@Temperature 30.0 °C
310 - 390 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D 785
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527
Elongation at Yield 5.0 %
5.0 %
ISO 527
Tensile Modulus 1.87 GPa
271 ksi
ISO 527
Flexural Strength 67.0 MPa
9720 psi
ISO 1783
Flexural Modulus 1.85 GPa
268 ksi
ISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Maximum Service Temperature, Air >= 180 °C
>= 356 °F
Exotherm Temp; Method 4
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ASTM D 648
Glass Transition Temp, Tg 155 °C
311 °F
Method 1
Smoke Density 1.33 - 1.66 min
1.33 - 1.66 min
At 30°C; Method 4
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
non show side
80.0 °C
176 °F
show side