Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an inherent static dissipative polymer network. This inherent static dissipative network remains intact through injection molding or extruding while maintaining the physical properties of TPU. Stat-Rite® TPU alloys are formulated for permanent and consistent ESD protection without comprising cleanliness. Features:Permanently static dissipativeDoes not require humidityUltra-Clean: low off-gassing, low ionics, low particulatesSee-through clarityNo particulatesApplications:Cleanroom soft walls, windows and doorsElectronic component handlingVacuum TubingWork surface matsProperties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. For best results, always dry the material two to three hours at 105°C (220°F) in a dehumidifying hopper dryer. Data provided by Noveon, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
100% Modulus 0.0103 GPa
1.50 ksi
ASTM D412
300% Modulus 0.0193 GPa
2.80 ksi
ASTM D412
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies transparent but doesn't quantify
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+10 ohm
1.00e+10 ohm
ASTM D257
Static Decay 0.20 sec
0.20 sec
50% R.H. Charge Plate Monitor
Processing Properties Metric English Comments
Drying Temperature 105 °C
221 °F
Dry Time 2 - 3 hour
2 - 3 hour
Descriptive Properties Value Comments
Color Transparent