Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Hipscon™ M-520 Static Control High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Lubrizol (former Noveon)
Trade Name Hipscon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Hipscon™ M-520 Static Control High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hipscon™ M-520 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are easily formed into deep pockets that maintain uniform static protection and show excellent "crush strength." Hipscon maintains extremely low gloss surfaces after forming, allowing for easy reading of package contents via automated sensors. Hipscon™ M-520 sheet is available in custom extruded gauges from 0.012 to 0.080 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finish. Features:Superior crush strengthHigh degree of stiffnessUniform pocket formationConsistent, permanent ESD protectionApplications:Electronic component packaging and handling traysTape & reelMaterial handling boxes and binsData provided by Noveon, Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.86 GPa
270 ksi
ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
Injection Molded; ASTM D790-92
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 12 %
12 %
60°; Front
12 %
12 %
60°; Back
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Surface Resistance <= 1e+05
<= 1e+05
ASTM D257
Static Decay <= 0.010 sec
<= 0.010 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
<= 0.010 sec
<= 0.010 sec
FTMS-101C; 12% R.H., (-5000 V to -50 V)
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: