Lubrizol Hipscon™ B-515 Static Control Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Lubrizol (former Noveon)
Trade Name Hipscon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Hipscon™ B-515 Static Control Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hipscon™ B-515 is a carbon black-filled, Polystyrene compound available in compound form. Hipscom™ B-515 compound maintains extremely low gloss surfaces after molding, allowing for easy reading of package contents via automated sensors. Features:High degree of stiffness Consistent, permanent ESD protectionHumidity independentApplications:Electronic component packaging and handling traysMaterial handling boxes and binsData provided by Noveon, Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.86 GPa
270 ksi
ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Surface Resistivity per Square <= 1e+05
<= 1e+05
ASTM D257
Static Decay <= 0.010 sec
<= 0.010 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
<= 0.010 sec
<= 0.010 sec
FTMS-101C; 12% R.H., (-5000 V to -50 V)
Descriptive Properties Value Comments
Color Black