Lubrizol Estane® CS190A Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® CS190A Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® CS190A is a Shore 90A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Ultimate 34.3 MPa
4980 psi
ASTM D412
Tensile Strength, Yield 6.37 MPa
925 psi
at 100% elongation; ASTM D412
11.3 MPa
1640 psi
at 300% elongation; ASTM D412
Elongation at Break 720 %
720 %
ASTM D412
Tear Strength 93.2 kN/m
532 pli
Die C; ASTM D624
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 °C
176 °F
ASTM D1525