Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 100 °C
10 g/10 min

@Load 4.76 lb,
Temperature 212 °F
ASTM D1230
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Dry; ASTM D2240
Tensile Strength, Ultimate 5.17 MPa
750 psi
Dry weak gel; ASTM D412
Elongation at Break 100 %
100 %
Dry weak gel; ASTM D412
Processing Properties Metric English Comments
Zone 1 100 °C
212 °F
Zone 2 105 °C
221 °F
Zone 3 110 °C
230 °F
Zone 4 115 °C
239 °F
Die Temperature 115 °C
239 °F
Melt Temperature 115 °C
239 °F
Drying Temperature 43.3 °C
110 °F
forced air desiccant dryer
Dry Time 4.00 hour
4.00 hour
Users viewing this material also viewed the following: