Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR E50D Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR E50D Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR E50D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Ultimate 57.2 MPa
8300 psi
ASTM D412
Elongation at Break 360 %
360 %
ASTM D412
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
200% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
300% Modulus 0.0386 GPa
5.60 ksi
ASTM D412
Flexural Modulus 0.0896 GPa
13.0 ksi
ASTM D790