Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR CL650 is an aliphatic, polycaprolactone-based TPU with a Shore D Durometer of 65.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin is clear, UV resistant, it will not discolor and has excellent mechanical properties.Uses: Outdoor applications, protective films and graphics.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 175 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 347 °F
ASTM D1230
Mechanical Properties Metric English Comments
Hardness, Shore D 65

@Time 5.00 sec
65

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 64.5 MPa
9350 psi
ASTM D412
Tensile Strength, Yield 22.4 MPa
3250 psi
at 100%; ASTM D412
28.6 MPa
4150 psi
at 200%; ASTM D412
Elongation at Break 340 %
340 %
ASTM D412
Flexural Modulus 0.379 GPa
55.0 ksi
ASTM D790
Users viewing this material also viewed the following: