Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® AG 9550 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® AG 9550 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® AG 9550 is a polyether based aliphatic polyurethane designed for flat die extrusion into film and sheet products.Features: Very tough, high modulus, high tear and tensile properties that will impart good impact resistance to bullet-resistant applications. Excellent impact and UV resistance.Uses: Designed for the lamination of glass to glass laminates with exposed edges.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.1 MPa
9000 psi
ASTM D412
Elongation at Break 375 %
375 %
ASTM D412
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
200% Modulus 0.0172 GPa
2.50 ksi
ASTM D412
300% Modulus 0.0296 GPa
4.30 ksi
ASTM D412
Tear Strength 77.1 kN/m
440 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
DSC
Optical Properties Metric English Comments
Refractive Index 1.499
1.499
ASTM D542-95
Haze 0.30 %
0.30 %
ASTM D1003
Yellow Index <= 1.0 %
<= 1.0 %
ASTM D1925
Transmission, Visible 90 %
90 %
ASTM D1003
Descriptive Properties Value Comments
TMA Peak (°C) 155
TMA Range (°C) 90-200