Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimSpecific Notes for this Material: Excellent extrusion, processability, low temperature flexibility, good clarity, substrate for overmolding Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
DIN 53505
Tensile Strength, Ultimate 33.0 MPa
4790 psi
DIN 53504
Elongation at Break 520 %
520 %
DIN 53504
50% Modulus 0.0113 GPa
1.64 ksi
DIN 53504
100% Modulus 0.0128 GPa
1.86 ksi
DIN 53504
300% Modulus 0.0202 GPa
2.93 ksi
DIN 53504
Flexural Stiffness 98.002 MPa
14214 psi
ASTM D747
Tear Strength 110 kN/m
628 pli
DIN 53515
Abrasion 75
75
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Vicat Softening Point 93.0 °C
199 °F
A50; DIN 53460
Descriptive Properties Value Comments
E-Modulus 87 mm/min
Users viewing this material also viewed the following: