Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Glass Filled
Manufacturer Lubrizol (former Noveon)
Trade Name ESTALOC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ISO 1183
Filler Content 10 %
10 %
Glass
10 %
10 %
Mineral
Maximum Moisture Content 0.020
0.020
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
flex bar; ASTM D955
0.0030 cm/cm
0.0030 in/in
average flow and against flow, disc; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 71 - 77

@Time 5.00 sec
71 - 77

@Time 0.00139 hour
ASTM D2240
Tensile Strength 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 39 %
39 %
ASTM D638
Tensile Modulus 1.90 GPa
276 ksi
ASTM D638
Flexural Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
ASTM D955
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
ASTM D955
Processing Properties Metric English Comments
Rear Barrel Temperature 199 °C
390 °F
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 221 °C
430 °F
Nozzle Temperature 227 °C
441 °F
Melt Temperature 227 °C
441 °F
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Injection Pressure 69.0 - 103 MPa
10000 - 14900 psi
Hold Pressure 35.0 - 69.0 MPa
5080 - 10000 psi
Back Pressure 0.345 MPa
50.0 psi
Screw Speed 30 - 80 rpm
30 - 80 rpm