Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTAGRIP® ST80A Polyether-Type Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTAGRIP®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTAGRIP® ST80A Polyether-Type Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83

@Time 5.00 sec
77 - 83

@Time 0.00139 hour
ASTM D2240
Tensile Strength 22.8 MPa
3310 psi
ASTM D412
Tensile Stress 3.70 MPa

@Strain 100 %
537 psi

@Strain 100 %
ASTM D412
6.70 MPa

@Strain 300 %
972 psi

@Strain 300 %
ASTM D412
Elongation at Break 750 %
750 %
ASTM D412
Graves Tear Strength 68.4 kN/m
390 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 45
45
H-18, 1000 g; ASTM D3389 B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -51.0 °C
-59.8 °F
by DSC
Processing Properties Metric English Comments
Rear Barrel Temperature 218 °C
424 °F
Middle Barrel Temperature 221 °C
430 °F
Front Barrel Temperature 227 °C
441 °F
Nozzle Temperature 227 °C
441 °F
Melt Temperature 227 °C
441 °F
pyrometer check of air shot