Lubrizol Advanced Materials Pearlthane® Maxi 12T85E Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® Maxi 12T85E Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLTHANE® MAXI 12T85E is a polyester based TPU, supplied in form of transparent, colorless pellets, featuring medium hardness, good mechanical properties and outstanding abrasion resistance. This grade is intended for extrusion applications.Information provided by Merquinsa.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ASTM D2240
Tensile Strength, Yield 42.08 MPa
6103 psi
ASTM D412
Elongation at Break 580 %
580 %
ASTM D412
100% Modulus 0.00591 GPa
0.857 ksi
ASTM D412
300% Modulus 0.01092 GPa
1.584 ksi
ASTM D412
Abrasion 30
30
[mm<sup>3</sup>]. Loss; ISO 4649
Thermal Properties Metric English Comments
Melting Point 180 - 190 °C
356 - 374 °F
MQSA 114
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC, 50°F/min; DIN 51.007
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44
Copyright © lookpolymers.com All Rights Reserved