Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlcoat®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLCOAT® Activa D198K is an aliphatic based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss aspect” on the final product surface after extrusion processing. Featuring low gel content as well as low temperature flexibility, it is ideally suited for extrusion or co-extrusion onto polar substrates.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength, Yield 25.05 MPa
3633 psi
ASTM D412
Elongation at Break 455 %
455 %
ASTM D412
100% Modulus 0.00581 GPa
0.843 ksi
ASTM D412
300% Modulus 0.01302 GPa
1.889 ksi
ASTM D412
Tear Strength 55.0 kN/m
314 pli
ASTM D624 (die C)
Abrasion 30
30
[mm^3]; DIN 53.516
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -33.3 °C
-28.0 °F
DIN 51.007
Processing Properties Metric English Comments
Zone 1 185 - 205 °C
365 - 401 °F
Zone 2 190 - 210 °C
374 - 410 °F
Zone 3 195 - 215 °C
383 - 419 °F
Zone 4 190 - 210 °C
374 - 410 °F
Die Temperature 185 - 205 °C
365 - 401 °F