Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlbondâ„¢ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization rate and a very high thermoplasticity level. It contains 67% of renewable material as certified according to ASTM-D6866.Application: Pearlbondâ„¢ ECO D590 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS (HMPUR), in order to improve the crystallisation speed.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Viscosity 1.68e+6 cP

@Temperature 130 °C
1.68e+6 cP

@Temperature 266 °F
Melt; ISO 1133
Melt Flow 30 - 60 g/10 min

@Load 2.16 kg,
Temperature 170 °C
30 - 60 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 80.0 - 84.0 °C
176 - 183 °F
MQSA 70 A
Processing Properties Metric English Comments
Moisture Content <= 0.150 %
<= 0.150 %
MQSA 44
Descriptive Properties Value Comments
Crystallization Rate 4-6 minutes
MQSA 12 B
OH Value < 3 mg/KOH/g
MQSA 47 A
Thermoplasticity Very High
MQSA 68A