Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® 11T65D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent mechanical properties.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ISO 868
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 2781
Tensile Strength, Yield 35.00 MPa
5076 psi
ISO 527-2/5A/500
Elongation at Break 440 %
440 %
ISO 527-2/5A/500
50% Modulus 0.00190 GPa
0.276 ksi
ISO 527-2/5A/500
100% Modulus 0.02501 GPa
3.628 ksi
ISO 527-2/5A/500
300% Modulus 0.03100 GPa
4.496 ksi
ISO 527-2/5A/500
Tear Strength 210 kN/m
1200 pli
ISO 34-1B
Abrasion 25
25
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 144 °C
291 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 225 °C
437 °F
Zone 1 220 °C
428 °F
Zone 2 225 °C
437 °F
Zone 3 230 °C
446 °F
Zone 4 230 °C
446 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F