Lubriplate SYN LUBE 32 PAO-Based Multi-Purpose Synthetic Fluid

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer Lubriplate Lubricants
Trade Name SYN LUBE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SYN LUBE 32 PAO-Based Multi-Purpose Synthetic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for many types of rotary screw and piston type air compressors, hydraulic systems, blowers, and turbine oil applications. Available in Pails and DrumsInformation provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 32
32
ISO Grade
136
136
Viscosity Index
Saybolt Viscosity at 100°F 160 SUS
160 SUS
Saybolt Viscosity at 210°F 47 SUS
47 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt
32 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Thermal Properties Metric English Comments
Pour Point -56.7 °C
-70.0 °F
Flammability Test 505
505
[°F] Fire Point
>= 700
>= 700
[°F] Auto-Ignition
Flash Point 243 °C
470 °F
Descriptive Properties Value Comments
SAE No. 10