Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubriplate SPO-266 Petroleum-Based Gear, Bearing, & Recirculating Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SPO-266 Petroleum-Based Gear, Bearing, & Recirculating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubrication for high sliding action in worm gears. They are also excellent for bevel, helical, and spur gears. They can be used with silver alloy, copper, and copper alloy bearings. Excellent for use in high moisture and high temperature applications. Provides performance comparable to synthetic lubricants. SPO Series Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 102
102
Viscosity Index
320
320
ISO Grade
Saybolt Viscosity at 100°F 1476 SUS
1476 SUS
Saybolt Viscosity at 210°F 115 SUS
115 SUS
Kinematic Viscosity at 40°C (104°F) 280 cSt
280 cSt
Kinematic Viscosity at 100°C (212°F) 23 cSt
23 cSt
Thermal Properties Metric English Comments
Pour Point -12.2 °C
10.0 °F
Flammability Test 570
570
[°F] Fire Point
Flash Point 243 °C
470 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 90
SAE No. 60