Lubriplate Minus 70 Petroleum-Based Heavy-Duty Hydraulic Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name Minus
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate Minus 70 Petroleum-Based Heavy-Duty Hydraulic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISO 15 petroleum-based oil for low temperature applications. Low Temp Hydraulic Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 15
15
ISO Grade
340
340
Viscosity Index
Saybolt Viscosity at 100°F 84 SUS
84 SUS
Saybolt Viscosity at 210°F 45 SUS
45 SUS
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Thermal Properties Metric English Comments
Pour Point -56.7 °C
-70.0 °F
Flammability Test 220
220
[°F] Fire Point
Flash Point 93.3 °C
200 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 75W
SAE No. 5W-20