Lubriplate 1240 Lithium-Polymer Type Multi-Purpose Grease

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 1240 Lithium-Polymer Type Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Highly water resistant and tacky, they are designed for applications were the grease is subjected to heavy pressure and shock loads. This series is available in 3 NLGI densities for a wide range of applications and temperatures. Applications: Centralized systems, const. industrial equip.1240 Series Greases are available in Cartridges, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1250 SUS
1250 SUS
Kinematic Viscosity at 40°C (104°F) 237 cSt
237 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 355
355
Unknown Amount of Work
Penetration P(60), 1/10 mm 385
385
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Approx. Cold test
Dropping Point 204 °C
400 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 0
Rust/Oxidative Additives YES
Water Resistant YES