Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Filler Content 20 %
20 %
30 %
30 %
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 - 80.0 MPa
10200 - 11600 psi
ASTM D683
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
ASTM D638
Flexural Modulus 4.00 - 4.50 GPa
580 - 653 ksi
ASTM D790
Izod Impact, Notched 0.800 - 1.00 J/cm
1.50 - 1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 - 145 °C
275 - 293 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Users viewing this material also viewed the following: