Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ASTM D683
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.500 - 0.600 J/cm
0.937 - 1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in