Lotus Nano Paint NAP 301 Airport Nano-paint

Category Fluid
Manufacturer Lotus Nano Paint
Trade Name NAP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotus Nano Paint NAP 301 Airport Nano-paint.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This grade of traffic marking nano-paints is a fast dry and has better reflection of light. Because of these specifications these paint are suitable for Airports and inter-city roads. This paint has better performance in traffic lots demonstration.Applications: Airport and inter-city roadsInformation provided by Lotus Nanopaint
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.60 g/cc
1.50 - 1.60 g/cc
ASTM D1475
Solids Content 50 - 54 %
50 - 54 %
by Volume
71 - 75 %
71 - 75 %
by Weight; ASTM D1644
Processing Properties Metric English Comments
Dry Time 0.167 hour

@Temperature 25.0 °C
0.167 hour

@Temperature 77.0 °F
ASTM D711
Descriptive Properties Value Comments
Color White and Yellow
ASTM EN 1439
Coverage 7.8 m2/Liter
ASTM D344
Curing Solvent Evaporation
Direction Reflectance ~60%
Colored, ASTM E97
0.9
White, ASTM E97
Gloss Opaque
Resin Acrylic
Skiing Resistance (SRT) Passes
ASTM EN 1436
Thinner Lotus 65 B
Water Resistance Passes
ASTM D870