Lotus Nano Paint NAP 201 Fast Dry Nano-paint

Category Fluid
Manufacturer Lotus Nano Paint
Trade Name NAP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotus Nano Paint NAP 201 Fast Dry Nano-paint.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: In some traffic marking it isn’t possible for us to close roads for long time because of traffic conditions. This paint dry fast and we can reduce the closing time of the road or avoid closing the roads.Applications: Highway and inter-city roadsInformation provided by Lotus Nanopaint
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.60 g/cc
1.50 - 1.60 g/cc
ASTM D1475
Solids Content 50 - 54 %
50 - 54 %
by Volume
71 - 75 %
71 - 75 %
by Weight; ASTM D1644
Processing Properties Metric English Comments
Dry Time 0.167 hour

@Temperature 25.0 °C
0.167 hour

@Temperature 77.0 °F
ASTM D711
Descriptive Properties Value Comments
Color White and Yellow
ASTM EN 1439
Coverage 7.9 m2/Liter
ASTM D344
Curing Solvent Evaporation
Direction Reflectance ~55%
Colored, ASTM E97
0.87
White, ASTM E97
Gloss Opaque
Resin Acrylic
Skiing Resistance (SRT) Passes
ASTM EN 1436
Thinner Lotus 65 B
Water Resistance Passes
ASTM D870