Lotus Nano Paint NAP 103 Nano-paint

Category Fluid
Manufacturer Lotus Nano Paint
Trade Name NAP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotus Nano Paint NAP 103 Nano-paint.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This product has more resistance in environment and surface temperature and cause to be more durable on the road. For tropical places this paint cause better traffic lots in long time.Applications: Urban and inter-cityInformation provided by Lotus Nanopaint
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.60 g/cc
1.50 - 1.60 g/cc
ASTM D1475
Solids Content 51 - 55 %
51 - 55 %
by Volume
73 - 77 %
73 - 77 %
by Weight; ASTM D1644
Processing Properties Metric English Comments
Dry Time 0.330 hour

@Temperature 25.0 °C
0.330 hour

@Temperature 77.0 °F
ASTM D711
Descriptive Properties Value Comments
Color White, Yellow, Red and Blue
ASTM EN 1439
Coverage 7.2 m2/Liter
ASTM D344
Curing Solvent Evaporation
Direction Reflectance ~55%
Colored, ASTM E97
0.86
White, ASTM E97
Gloss Opaque
Resin Acrylic
Skiing Resistance (SRT) Passes
ASTM EN 1436
Thinner Lotus 65 B
Water Resistance Passes
ASTM D870