Lotus Nano Paint NAP 101 Nano-paint

Category Fluid
Manufacturer Lotus Nano Paint
Trade Name NAP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotus Nano Paint NAP 101 Nano-paint.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Traffic marking nano-paints improved with nano-particles to get better performance in traffics on the road. Better mechanical properties, excellent traffic performance and more durability on the road are the results of applying nanotechnology in traffic marking paints.Applications: Urban and inter-cityInformation provided by Lotus Nanopaint
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.60 g/cc
1.50 - 1.60 g/cc
ASTM D1475
Solids Content 51 - 55 %
51 - 55 %
by Volume
73 - 77 %
73 - 77 %
by Weight; ASTM D1644
Processing Properties Metric English Comments
Dry Time 0.330 hour

@Temperature 25.0 °C
0.330 hour

@Temperature 77.0 °F
ASTM D711
Descriptive Properties Value Comments
Color White, Yellow, Red and Blue
ASTM EN 1439
Coverage 8.7 m2/Liter
ASTM D344
Curing Solvent Evaporation
Direction Reflectance ~55%
Colored, ASTM E97
0.86
White, ASTM E97
Gloss Opaque
Resin Acrylic
Skiing Resistance (SRT) Passes
ASTM EN 1436
Thinner Lotus 65 B
Water Resistance Passes
ASTM D870