Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LI5011 is a pelleted high flow linear low density polyethylene. The higher melting point of the resin allows for higher end-use temperatures.Applications: House-wares, toys, lids, containers.Advantages: Outstanding stress crack resistance, excellent low temperature toughness, excellent mold ability, superior gloss and low odor.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
ESCR 100% Igepal® 4.0 hour

@Thickness 3.80 mm,
Temperature 50.0 °C
4.0 hour

@Thickness 0.150 in,
Temperature 122 °F
non slit; ASTM D1693
Base Resin Melt Index 50 g/10 min
50 g/10 min
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.7 MPa
1990 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
1% Secant Modulus 343.23 MPa
49782 psi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
resin; ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 170 - 220 °C
338 - 428 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F