Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down ability.Applications: Rice bags, shipping sacks, industrial liners.Advantages: Outstanding puncture strength, impact strength and tear strength.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 25.0 microns
0.984 mil
extruded at 2:1 BUR
Base Resin Melt Index 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 15.0 g/micron
381 g/mil
ASTM D1922
Dart Drop 4.00 g/micron
102 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 40.2 MPa
5830 psi
ASTM D882
Film Tensile Strength at Break, TD 30.4 MPa
4410 psi
ASTM D882
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
1% Secant Modulus, TD 196.14 MPa
28447 psi
ASTM D882
Optical Properties Metric English Comments
Haze 16 %
16 %
ASTM D1003
Gloss 60 %
60 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 180 - 200 °C
356 - 392 °F
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0