Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down ability.Applications: Thin film, agriculture film, ice bags, heavy duty bags, industrial packaging, liners.Advantages: Outstanding puncture strength, impact strength and tear strength.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.922 g/cc
0.0333 lb/in³
ASTM D1505
Thickness 25.0 microns
0.984 mil
extruded at 2:1 BUR
Base Resin Melt Index 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 18.0 g/micron
457 g/mil
ASTM D1922
Dart Drop 4.00 g/micron
102 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 40.2 MPa
5830 psi
ASTM D882
Film Tensile Strength at Break, TD 30.4 MPa
4410 psi
ASTM D882
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
1% Secant Modulus, TD 196.14 MPa
28447 psi
ASTM D882
Optical Properties Metric English Comments
Haze 17 %
17 %
ASTM D1003
Gloss 50 %
50 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 180 - 200 °C
356 - 392 °F
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0
Users viewing this material also viewed the following: