Lord Adhesives Thermosetâ„¢ MT-220 Thermally Conductive Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Thermoset™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Thermosetâ„¢ MT-220 Thermally Conductive Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LORD Thermosetâ„¢ MT-220 thermally conductive adhesive is a fast cure, one-component adhesive designed for use as a thermal interface adhesive for heat sink attachment and other applications requiring superior adhesion strength and extremely high thermal conductivity.All information provided by Lord.
Physical Properties Metric English Comments
Specific Gravity 2.49 g/cc
2.49 g/cc
Brookfield Viscosity 45000 cP

@Temperature 25.0 °C
45000 cP

@Temperature 77.0 °F
Spindle 6 @ 10rpm
100000 cP

@Temperature 25.0 °C
100000 cP

@Temperature 77.0 °F
Spindle 6 @ 1rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
Modulus of Elasticity 0.156 GPa
22.6 ksi
Storage
Shear Strength 6.21 MPa

@Temperature 900.45 °C
900 psi

@Temperature 1652.8 °F
Lap
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
Alpha 1
82.0 µm/m-°C
45.6 µin/in-°F
Alpha 2
Thermal Conductivity 4.20 W/m-K
29.1 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg -90.0 °C
-130 °F
TMA
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
30.0 min

@Temperature 125 °C
0.500 hour

@Temperature 257 °F
Pot Life 10080 min

@Temperature 25.0 °C
10080 min

@Temperature 77.0 °F
Shelf Life 6.00 Month

@Temperature -40.0 °C
6.00 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Appearance Gray
Consistency Paste