Material Notes:
LORD Thermosetâ„¢ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing application equipment.Thermoset MD-150 adhesive provides excellent adhesion to a wide variety of surfaces including silicon, silver, gold and copper. Low ionic levels make it ideally suited for demanding semiconductor and hybrid assembly applications.All information provided by Lord.
Physical Properties Metric English Comments
Specific Gravity 3.50 g/cc
3.50 g/cc
Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Modulus of Elasticity 5.00 GPa

@Temperature 25.0 °C
725 ksi

@Temperature 77.0 °F
Storage
Shear Strength 41.4 MPa

@Temperature 25.0 °C
6000 psi

@Temperature 77.0 °F
Die
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C
30.0 µin/in-°F
Alpha 1
160 µm/m-°C
88.9 µin/in-°F
Alpha 2
Glass Transition Temp, Tg 93.0 °C
199 °F
TMA
Component Elements Properties Metric English Comments
Potassium, K 0.0010 %
0.0010 %
Sodium, Na 0.0050 %
0.0050 %
Electrical Properties Metric English Comments
Volume Resistivity 0.000080 ohm-cm

@Temperature 25.0 °C
0.000080 ohm-cm

@Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 175 °C
1.00 hour

@Temperature 347 °F
Shelf Life 6.00 Month

@Temperature -40.0 °C
6.00 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Appearance Silver
Chloride (%) 0.005
Consistency Paste