Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition

Category Ceramic , Glass , Glass Ceramic
Manufacturer Lord Adhesives
Trade Name Metech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dielectric composition 7600A is a glass-ceramic insulative film designed for use in high density multilayer hybrid circuits using either gold or palladium-silver conductors. 7600A fires at 850°C to a smooth, dense, blue colored film that matches the thermal coefficient of expansion of alumina. Top gold conductor layers of Metech 3610 and 3612 exhibit excellent wire bonding using both aluminum and gold wire respectively. Top conductor layers of 3615 platinum-gold and 3504 palladium-silver display excellent solderability and aged adhesion.All information provided by Lord.
Physical Properties Metric English Comments
Brookfield Viscosity 170000 - 190000 cP

@Temperature 25.0 °C
170000 - 190000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Thickness 34.0 - 45.0 microns
1.34 - 1.77 mil
Fired
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
at 100VDC
Dielectric Constant 8.0 - 11

@Frequency 1000 Hz
8.0 - 11

@Frequency 1000 Hz
Dielectric Breakdown >= 600 V
>= 600 V
AC; 25 microns
Dissipation Factor <= 0.25

@Frequency 1000 Hz
<= 0.25

@Frequency 1000 Hz
Descriptive Properties Value Comments
Coverage (cm²/gm) 65-75
Calculated from 50 micron wet film
Via Resolution (microns) 200-250