Lord Adhesives Flocklok® 550P Flock Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Flocklok®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Flocklok® 550P Flock Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LORD Flocklok® 550P adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of uncured and semi-cured elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good resistance to abrasion. Flocklok 550P flock adhesive will react and cure with moisture; however, an elevated temperature cure is required to optimize adhesion and performance properties.All information provided by Lord.
Physical Properties Metric English Comments
Density 1.0425 - 1.0904 g/cc
0.037663 - 0.039393 lb/in³
Solids Content 70 - 74 %
70 - 74 %
Viscosity 125 - 500 cP

@Temperature 25.0 °C
125 - 500 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point 44.0 °C
111 °F
Seta
Processing Properties Metric English Comments
Cure Time 1.00 - 3.00 min

@Temperature 204 - 260 °C
0.0167 - 0.0500 hour

@Temperature 399 - 500 °F
Descriptive Properties Value Comments
Appearance Brown Liquid
Solvents N-Butyl Propionate