Material Notes:
Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.850 g/cc
0.0307 lb/in³
9924V; ASTM D1475-85
0.960 g/cc
0.0347 lb/in³
Mixed; ASTM D1475-85
1.10 g/cc
0.0397 lb/in³
9924A; ASTM D1475-85
Solids Content 0.00 %
0.00 %
9924V; by weight; ASTM D2369-87 Modified
11 %
11 %
Mixed; by volume; ASTM D2369-87 Modified
18.2 %
18.2 %
Mixed; by weight; ASTM D2369-87 Modified
33 %
33 %
9924A; by weight; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 679 g/l
679 g/l
9924A; ASTM D3960-87
773 g/l
773 g/l
Mixed; ASTM D3960-87
830 g/l
830 g/l
9924V; ASTM D3960-87
Brookfield Viscosity 225 cP
225 cP
Mixed; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
3000 cP
3000 cP
9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
10 cP

@Temperature 25.0 °C
10 cP

@Temperature 77.0 °F
9924V; ASTM D2196-66; LVT, Spindle #1 @ 60rpm
Viscosity Measurement 11 - 15
11 - 15
seconds; Zahn, #4 cup
48 - 52
48 - 52
seconds; Zahn, #2 cup
Mechanical Properties Metric English Comments
Impact Test 18.1 J
13.3 ft-lb
Direct; Gardner
18.1 J
13.3 ft-lb
Reverse; Gardner
Thermal Properties Metric English Comments
Flash Point 19.0 °C
66.2 °F
9924A; Setaflash, Closed Cup; ASTM D3278-82
20.6 °C
69.1 °F
9924V; Setaflash, Closed Cup; ASTM D3278-82
Processing Properties Metric English Comments
Dry Time 0.33 hour

@Temperature 22.2 °C
0.33 hour

@Temperature 72.0 °F
Set to touch; Gardner, Mechanical
1 hour

@Temperature 22.2 °C
1 hour

@Temperature 72.0 °F
Surface Dry; Gardner, Mechanical
2 hour

@Temperature 22.2 °C
2 hour

@Temperature 72.0 °F
Dry Hard; Gardner, Mechanical
Pot Life 480 min
480 min
Shelf Life 12.0 Month
12.0 Month
9924V
6.00 Month

@Temperature <=26.7 °C
6.00 Month

@Temperature <=80.1 °F
9924A
Descriptive Properties Value Comments
Appearance Clear, colorless to straw
9924V
Red
Mixed
Red
9924A
Conical Mandrel Bend Passes 1/8"
ASTM D522
Mix Ratio 1:1
by volume
8.8:8.8
by weight