Material Notes:
Aeroglaze® 9924 wash primer was designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
9924B; ASTM D1475-85
0.990 g/cc
0.0358 lb/in³
Mixed; ASTM D1475-85
1.10 g/cc
0.0397 lb/in³
9924A; ASTM D1475-85
Solids Content 0.00 %
0.00 %
9924B; by weight; ASTM D2369-87 Modified
11 %
11 %
Mixed; by volume; ASTM D2369-87 Modified
17.4 %
17.4 %
Mixed; by weight; ASTM D2369-87 Modified
33 %
33 %
9924A; by weight; ASTM D2369-87 Modified
Volatile Organic Compounds (VOC) Content 679 g/l
679 g/l
9924A; ASTM D3960-87
803 g/l
803 g/l
Mixed; ASTM D3960-87
928 g/l
928 g/l
9924B; ASTM D3960-87
Brookfield Viscosity 225 cP
225 cP
Mixed; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
3000 cP
3000 cP
9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm
10 cP

@Temperature 25.0 °C
10 cP

@Temperature 77.0 °F
9924B; ASTM D2196-66; LVT, Spindle #1 @ 60rpm
Viscosity Measurement 11 - 15
11 - 15
seconds; Zahn, #4 cup
48 - 52
48 - 52
seconds; Zahn, #2 cup
Mechanical Properties Metric English Comments
Impact Test 18.1 J
13.3 ft-lb
Direct; Gardner
18.1 J
13.3 ft-lb
Reverse; Gardner
Thermal Properties Metric English Comments
Flash Point 19.0 °C
66.2 °F
9924A; Setaflash; ASTM D3278-82
19.0 °C
66.2 °F
9924B; Setaflash; ASTM D3278-82
Processing Properties Metric English Comments
Dry Time 0.33 hour

@Temperature 22.2 °C
0.33 hour

@Temperature 72.0 °F
Set to touch; Gardner, Mechanical
1 hour

@Temperature 22.2 °C
1 hour

@Temperature 72.0 °F
Surface Dry; Gardner, Mechanical
2 hour

@Temperature 22.2 °C
2 hour

@Temperature 72.0 °F
Dry Hard; Gardner, Mechanical
Pot Life 480 min
480 min
Shelf Life 12.0 Month
12.0 Month
9924B
6.00 Month

@Temperature <=26.7 °C
6.00 Month

@Temperature <=80.1 °F
9924A
Descriptive Properties Value Comments
Appearance Clear, colorless to straw
9924B
Red
Mixed
Red
9924A
Conical Mandrel Bend Passes 1/8"
ASTM D522
Mix Ratio 1:1
by volume
8.8:8
by weight