Lord Adhesives 7713 Adhesion Increaser to SMC

Category Polymer , Adhesive , Thermoset
Manufacturer Lord Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives 7713 Adhesion Increaser to SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surface modifiers. Lord® Adhesion Enhancers/Surface Modifiers improve adhesion on virtually any hard-to-bond surface--whether you are joining metals, plastics, ceramics or elastomers.Lord Adhesives 7713 Adhesion Increaser to SMCSingle-component layover primer. Purple liquid. Specifically formulated to provide increased adhesion of adhesives to SMC. Trichloroethylene Methylene Chloride solvents. Non-volatile weight by content = 13.5-13.9%
Physical Properties Metric English Comments
Density 1.34 - 1.39 g/cc
0.0485 - 0.0502 lb/in³
Viscosity 20 cP
20 cP
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F