Loctite® Gasket Eliminator® 504 Flange Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name Gasket Eliminator®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Gasket Eliminator® 504 Flange Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic GasketingLoctite® 504 Gap Filling Rigid Cure Gasket Eliminator® Flange SealantA single-component, instant low pressure seal that fills gaps to 0.030". Typical Use: Gap filling
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Viscosity 500000 - 1.20e+6 cP
500000 - 1.20e+6 cP
Thixotropic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 - 240 min
0.500 - 4.00 hour
Full Cure; Primed
240 - 1440 min
4.00 - 24.0 hour
Full Cure; Unprimed
Descriptive Properties Value Comments
Color Orange
Gap Fill 0.030 in.
Unprimed
0.05 in.
Primed