Loctite® Durabond® U-05FL Urethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Loctite
Trade Name Durabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Durabond® U-05FL Urethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.Loctite® U-05FL Metal bonder, highly flexible, high peel, high shear Durabond® Urethane AdhesiveA two-part, high-performance urethane adhesive for metal bonding with a 5-minute worklife. Off-white, highly flexible, impact resistant, high peel, high sheer.Mix Ratio by Volume, Resin:Hardener = 1:2 Bonding Type: Urethane
Physical Properties Metric English Comments
Viscosity 640 cP
640 cP
Mixed - low; Resin - 640 cP; Hardener - 35,000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
Adhesive Bond Strength 6.89 - 20.7 MPa
1000 - 3000 psi
Varies with substrates
Peel Strength 0.877 - 5.26 kN/m
5.00 - 30.0 pli
Varies with substrates.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 48.0 °C
118 °F
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Test run on 1/8" specimens.
Processing Properties Metric English Comments
Pot Life 5.0 min
5.0 min
Descriptive Properties Value Comments
Color Off-white