Loctite® Durabond® E-214HP Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Loctite
Trade Name Durabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Durabond® E-214HP Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.Loctite® E-214HP High strength, temperature resistant, non-sag Durabond® Epoxy AdhesiveA one-component, heat cure epoxy. Grey, temperature resistant, high strength, non-sag.
Physical Properties Metric English Comments
Viscosity 150000 cP
150000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 20.7 - 41.4 MPa
3000 - 6000 psi
Varies with substrates
Peel Strength 5.26 - 12.3 kN/m
30.0 - 70.0 pli
Varies with substrates.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 120 °C
248 °F
Electrical Properties Metric English Comments
Dielectric Strength 21.7 kV/mm
550 kV/in
Test run on 1/8" specimens.
Descriptive Properties Value Comments
Color Grey