Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® Assure™ 425 Threadlocker

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name Assure™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Assure™ 425 Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from delicate electronic components to heavy construction equipment.Loctite® Pre-Applied Threadlockers are dry-to-the-touch films applied to threaded fasteners by fastener suppliers and process centers located throughout North America. Ideally suited for OEMs, they improve speed of assembly and ensure quality by eliminating on-line adhesive dispensing.Loctite® Threadlockers are available in varying viscosities and strengths for virtually any application, including exposure to extreme environments.Loctite® 425 Surface Curing Assure™ ThreadlockerLow strength, fast curing threadlocker for plastic fasteners. Can be applied before or after assembly.Torque capability, M10 steel nuts and bolts: 5 in. lbs. (break), 4 in. lbs. (prevail) Typical Use: For small plastic fasteners
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Viscosity 60 cP
60 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 2.00 min
0.0333 hour
840 min

@Temperature 25.0 °C
14.0 hour

@Temperature 77.0 °F
Full Cure; Steel
Descriptive Properties Value Comments
Color Blue
Copyright © lookpolymers.com All Rights Reserved