Loctite® 7360 Aliphatic Ester Blend Solvent Type Surface Mount Adhesive Solvent (Cleaner)

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 7360 Aliphatic Ester Blend Solvent Type Surface Mount Adhesive Solvent (Cleaner).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application techniques including syringe dispense, stencil print and pin transfer.Loctite® syringe dispense products provide good performance for electronics assembly:High Speed DispenseLow Temperature CureProducts for difficult-to-bond substratesLoctite® 7360 Aliphatic Ester Blend Solvent Type Surface Mount Adhesive Solvent (Cleaner)For clean-up and removal of uncured surface mount adhesive. No corrosive properties, No Ozone depletion potential.
Thermal Properties Metric English Comments
Flash Point 100 °C
212 °F