Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically Conductive Bonders and Gasketing and Wire TackersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditional methods such as solder, are not practical. Electrically Conductive Adhesives are ideal for attaching temperature sensitive components, or providing electrical interconnections on non-solderable substrates, such as plastic and glass.Loctite offers a complete line of electrically conductive adhesives to meet almost any need including: flexible, heat cure, room temperature cure, screen printable, high adhesion, and rapid cure.Loctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazards. Loctite offers both Form-in-place (FIP) and Cure-in-Place (CIP) compression gasket materials.Loctite® Tak Pak Adhesives are used to secure wires to printed circuit board assemblies. The fast cure times of these adhesives help increase the throughput of the wire tacking assembly process.Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone SealantProvides a resilient ground path for sensitive electronic devices. A non-corrosive form-in-place electrically conductive silicone that provides a ground path for sensitive electronic devices. Black paste heat cures in minutes to form a resilient seal. Volume resistivity is 150 O-cm. Cure Type: Heat Bonding Type: Silicone
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Ultimate 3.28 MPa
475 psi
Elongation at Break 125 %
125 %
Electrical Properties Metric English Comments
Volume Resistivity 150 ohm-cm
150 ohm-cm
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
5 min. @ 150ºC
Shelf Life 3.00 Month
3.00 Month
shelf life at 5ºC
Descriptive Properties Value Comments
Color Black
Extrusion Rate 350 g/min
1/8" orifice at 90 psi