Loctite® 5140 RTV Potting

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 5140 RTV Potting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies. For electronics assembly, Loctite offers deep potting, high adhesion, non-corrosive, and thermally conductive potting products. These can be cured with heat, UV light, or moisture.Loctite® 5140 RTV PottingA non-corrosive, UV curing silicone for high-speed shallow potting, coating and sealing of electronic devices, especially for military, automotive and industrial electronics. Meets Mil-A-46146B. Cure Type: Moisture Bonding Type: Silicone
Physical Properties Metric English Comments
Viscosity 35000 cP
35000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Full Cure
Gel Time >= 180 min
>= 180 min
Until skin over