Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® 3888 Room Temperature Cure Isotropic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3888 Room Temperature Cure Isotropic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditional methods such as solder, are not practical. Electrically Conductive Adhesives are ideal for attaching temperature sensitive components, or providing electrical interconnections on non-solderable substrates, such as plastic and glass.Loctite offers a complete line of electrically conductive adhesives to meet almost any need including: flexible, heat cure, room temperature cure, screen printable, high adhesion, and rapid cure.Loctite® 3888 Room Temperature Cure Isotropic Epoxy AdhesiveA room temperature cure adhesive for applications requiring a combination of good mechanical and electrical properties. Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 6.89 MPa
>= 1000 psi
Aluminum to Aluminum
Thermal Properties Metric English Comments
CTE, linear >= 50.0 µm/m-°C

@Temperature 20.0 °C
>= 27.8 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 50.0 °C
122 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0010 ohm-cm
<= 0.0010 ohm-cm
Processing Properties Metric English Comments
Cure Time 30.0 min
0.500 hour
24 hrs. @ 23ºC, 1 hr. @ 125ºC, 30 min. @ 150ºC
Pot Life 90.0 min

@Temperature 23.0 °C
90.0 min

@Temperature 73.4 °F