Material Notes:
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond. Bonding Type: Acrylic Typical Use: High temperature applications
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Viscosity 200000 cP
200000 cP
at 20 RPM
Mechanical Properties Metric English Comments
Adhesive Bond Strength 24.1 MPa
3500 psi
Varies with substrates
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 3.00 min
0.0500 hour
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Color Pale yellow
Gap Fill 0.02 in.